===== Failed Weld - possible bad weld wire (filler metal) or low amperage ===== | ===== Failed Weld - possible bad weld wire (filler metal) or low amperage ===== | ||
- | === == August 17, 2014 == === | + | ===== August 17, 2014 ===== |
**JP:** Quality welding wire makes a HUGE difference! I was shocked at the difference in splatter, arc striking, and porosity.... You should apologize to your bed rails right now. | **JP:** Quality welding wire makes a HUGE difference! I was shocked at the difference in splatter, arc striking, and porosity.... You should apologize to your bed rails right now. |